Physical Properties Metric English Comments
Water Vapor Transmission 6.70 g/m²/day
0.431 g/100 in²/day
ASTM F1249
Eastman Embrace LV Copolyester for Extruded/Cast Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Water Vapor Transmission 6.70 g/m²/day
0.431 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 75 CSR-2 OPP Film
Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.Availability: Latin America, North America and ..
Water Vapor Transmission 6.70 g/m²/day
0.431 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 75 SLP OPP Film
Product Description: Bicor SLP is a one-side treated, non-heat sealable OPP film designed for use as the outside web of a lamination. The treated print surface is intended as the print and laminatin..
Water Vapor Transmission 6.70 g/m²/day
0.431 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
ExxonMobil Bicor® 85 LTSC OPP Film
Product Description: Bicor LTSC is a two-side coated OPP film which is designed for use in high-speed or demanding horizontal, fin seal, packaging applications. The low-temperature seal coating (LTS..