Polymer Property : Water Vapor Transmission = 0.322 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 3.00 - 5.00 g/m²/day

@Thickness 0.300 mm,
Temperature 38.0 °C
0.193 - 0.322 g/100 in²/day

@Thickness 0.0118 in,
Temperature 100 °F
90% RH; ISO 62
Total PS CPDS 9217 Compound Polystyrene/Polyethylene
POLYSTYRENE (PS) COMPOUND (CPDS) 9217 is an alloy of polystyrene and polyethylene. This combination brings the benefits of polyethylene; a high level of stress crack resistance, mechanical properti..