Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.155 g/m²/day | 0.00998 g/100 in²/day | 86°F (30°C) / 60%RH; ASTM F1249 |
Honeywell ACLAR® CX 130E Heat Sealable PCTFE Film
(discontinued **) Description: ACLAR® CX 130E is a heat sealable PCTFE film with outstanding clarity. It is used where applications require moisture protection.Information provided by Honeywell. |