Water Vapor Transmission | 1.55 g/m²/day | 0.0998 g/100 in²/day | ASTM D3833 |
3M Scotch™ 2228 Rubber Mastic Tape 3M™ Scotch™ 2228 is a conformable self-fusing rubber electrical insulating sealing tape. Scotch 2228 consist of an ethylene propylene rubber (EPR) backing coated with an aggressive, temperature-st.. |