Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0930 g/m²/day | 0.00599 g/100 in²/day | 86°F (30°C) / 60%RH; ASTM F1249 |
Honeywell ACLAR® Rx 160 CTFE Homopolymer, Barrier Film Description: Aclar® Rx160 is a 0.60 mil (15 micron) PCTFE homopolymer, high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packag.. |