Polymer Property : Water Vapor Transmission = 0.0500 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.776 g/m²/day

@Temperature 38.0 °C
0.0500 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
DuPont Teijin Films Mylar® OB13AF Polyester Film, 100 Gauge
Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s..
Water Vapor Transmission 0.776 g/m²/day

@Temperature 38.0 °C
0.0500 g/100 in²/day

@Temperature 100 °F
90% RH; ASTM F1249
DuPont Teijin Films Mylar® OB13AF Polyester Film, 150 Gauge
Product Description: Mylar® OB13AF is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opposite s..