Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0500 g/m²/day | 0.00322 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 33C (7.80 mil) Copolymer Film
(discontinued **) Description: ACLAR® 33C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). 33C is used for military and industrial packaging applications.Information provided by Honeywell.. |
|||
Water Vapor Transmission | 0.0500 g/m²/day | 0.00322 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |