Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0370 g/m²/day | 0.00238 g/100 in²/day | 77°F (25°C) / 60%RH; ASTM F1249 |
Honeywell ACLAR® Rx20E CTFE Homopolymer, Barrier Film Description: ACLAR® Rx20Eis a .8 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipment.Inf.. |