Polymer Property : Water Vapor Transmission = 0.0219 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.340 g/m²/day
0.0219 g/100 in²/day
100°F (37.8°C) / 100%RH; ASTM F1249
Honeywell ACLAR® 22A (1.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22A is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It is a flexible transparent film used to package moisture sensitive products.Information provide..