Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.120 g/m²/day | 0.00773 g/100 in²/day | 100°F (37.8°C) / 100%RH; ASTM F1249 |
Honeywell ACLAR® 11A (2.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |