Polymer Property : Water Vapor Transmission = 0.00161 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 0.0250 g/m²/day
0.00161 g/100 in²/day
86°F (30°C) / 60%RH; ASTM F1249
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film
Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme..
Water Vapor Transmission 0.0250 g/m²/day

@Thickness 1.00 mm,
Temperature 23.0 °C
0.00161 g/100 in²/day

@Thickness 0.0394 in,
Temperature 73.4 °F
85% RH; DIN 53122
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..