Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0120 g/m²/day | 0.000773 g/100 in²/day | 77°F (25°C) / 60%RH; ASTM F1249 |
Honeywell ACLAR® UltRx 3000 CTFE Homopolymer, Barrier Film Description: ACLAR® UltRx 3000 is a 3 mil CTFE homopolymer high performance barrier film for the pharmaceutical and medical markets. It thermoforms well on conventional blister packaging equipme.. |