Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Transmission | 0.0000250 - 0.250 g/m²/day | 0.00000161 - 0.0161 g/100 in²/day | Average value: 0.111 g/m²/day Grade Count:8 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Water Vapor Transmission | 0.0000250 g/m²/day @Temperature 23.0 °C |
0.00000161 g/100 in²/day @Temperature 73.4 °F |
85% RH; DIN 53122 |