Polymer Property : Neck In = 4.02 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Neck In 10.2 cm

@Temperature 295 °C
4.02 in

@Temperature 563 °F
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate
Product Description: Product Description: Optema TC 220 is an ethylene methyl acrylate copolymer, which can be used for making alloys, blends and compounds or be injection molded where softness and ..