Physical Properties Metric English Comments
Neck In 3.30 cm

@Temperature 315 °C
1.30 in

@Temperature 599 °F
82 ft/min, Constant output at 35 rpm; ExxonMobil Method
ExxonMobil LDPE LD 250 Low Density Polyethylene Resin (European Grade)
Product Description: LD 250 is an LDPE extrusion coating grade, especially designed for low speed extrusion coating applications providingvery low neck-in characteristicsgood heat sealing properties..