Physical Properties Metric English Comments
Carbon Dioxide Transmission 450 cc-mm/m²-24hr-atm

@Thickness 0.100 mm
1140 cc-mil/100 in²-24hr-atm

@Thickness 0.00394 in
4500 cc/m²-24hr-bar; film; b.o. ISO 2556
Covestro Makrolon® 2256 Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•..