Physical Properties | Metric | English | Comments |
---|---|---|---|
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
630 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
160 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
630 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
160 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
630 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
160 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
630 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.100 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00394 in |
160 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Nitrogen Transmission | 16.0 cc-mm/m²-24hr-atm @Thickness 0.0254 mm |
40.6 cc-mil/100 in²-24hr-atm @Thickness 0.00100 in |
630 cc/m²-24hr-bar; film; b.o. ISO 2556 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |