Vapor Pressure 0.357 bar
268 torr
3M Fluorinert™ FC-3284 Electronic Liquid
3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test..