Physical Properties Metric English Comments
Vapor Pressure 0.0293 bar

@Temperature 20.0 °C
22.0 torr

@Temperature 68.0 °F
Vapor Density=3.14
LG Chemical Toluene
Colorless liquid with benzene odor, Heavier than air and highly inflammable, and Not soluble to water, Readily soluble in alcohol and etherStructure & Characteristics: C6H5CH3. Synthesized by extrac..