Physical Properties Metric English Comments
Vapor Pressure 0.133 bar

@Temperature 25.0 °C
100 torr

@Temperature 77.0 °F
Solvay Specialty Polymers PERFLUOROSOLVâ„¢ PFS1 Perfluorinated Cleaning Solvent
PERFLUOROSOLV PFS-1 is a low molecular weight perfluoropolyether solvent and diluent that perfroms well in many electronic and semiconductor cleaning functions, such as: pump cleaning, degreasing, d..
Vapor Pressure 0.133 bar

@Temperature 20.0 °C
100 torr

@Temperature 68.0 °F
ExxonMobil Method
ExxonMobil Exxsol™ DSP 70/90 Dearomatized Fluid
Availability: South America Appearance: Clear/Transparent LiquidInformation provided by ExxonMobil