Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.00192 bar | 1.44 torr | |
3M Fluorinert™ FC-43 Electronic Liquid 3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct.. |