Physical Properties Metric English Comments
Vapor Pressure 0.699 - 1.20 bar
524 - 897 torr
Unipetrol C5 Fraction
C5 fraction is mixture of mainly alifatic and cyclic hydrocarbons C5. It is colourless, volatile, extremely combustible and easily inflammable liquid with characteristic odour. It generates as a by-..