Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 1.00e-6 bar | 0.000750 torr | |
BASF 2- Ethylhexyl Acrylate Formula: C11H20O2CAS: 203-080-7Description: Acrylic ester for manufacturing polymers and for use as a feedstock for syntheses. Applications: 2-Ethylhexyl acrylate forms homopolymers and copolymers. .. |