Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.145 bar | 109 torr | |
3M Novec™ 7200 Engineered Fluid 3M™ Novec™ 7200 fluid's convenient boiling point and excellent environmental, health and safety profile make it useful as a heat transfer fluid, cleaning solvent, for lubricant deposition & many m.. |
|||
Vapor Pressure | 0.145 bar | 109 torr | |
3M Novec™ 8200 Engineered Fluid 3M™ Novec™ 8200 Engineered Fluid is a clear, colorless, low-odor fluid intended to replace 1,1,1-trichloroethane and perchloroethylene in film cleaning applications.Features and Benefits:Zero ozon.. |