Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000133 bar @Temperature 200 °C |
0.0998 torr @Temperature 392 °F |
|
PolyOne Synplast™ TOTM-E Tri (2-ethylhexyl) Trimellitate Branched C8 trimellitate ester with antioxidantContains 0.10-0.15 wt% 1,1,3-Tris (2-methyl-4hydroxy-5-t-butyl phenyl) butane antioxidantInformation provided by PolyOne |