Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0000333 bar @Temperature 25.0 °C |
0.0250 torr @Temperature 77.0 °F |
|
Solvay Specialty Polymers Galden® HT230 PFPE Heat Transfer Fluid Galden® HT grades are specifically recommended for use as heat transfer fluids.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service.. |