Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.0200 bar | 15.0 torr | |
Parker Chomerics CHO-FLEX 602B Catalyst Information provided by Chomerics |
|||
Vapor Pressure | 0.0200 bar @Temperature 20.0 °C |
15.0 torr @Temperature 68.0 °F |
|
Parker Chomerics CHO-SHIELD® 4991 Part B Conductive Coating Information provided by Chomerics |
|||
Vapor Pressure | 0.0200 bar @Temperature 20.0 °C |
15.0 torr @Temperature 68.0 °F |
|
Parker Chomerics CHO-SHIELD® 4995 Part B Conductive Coating Information provided by Chomerics |
|||
Vapor Pressure | 0.0200 bar @Temperature 20.0 °C |
15.0 torr @Temperature 68.0 °F |
|
Parker Chomerics CHO-SHIELD® 4997 Part B Conductive Coating Information provided by Chomerics |