Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000 bar @Temperature 25.0 °C |
0.000 torr @Temperature 77.0 °F |
|
BASF AH-Salt Recommended use: For the production of homopolymerisates and copolymerisatesInformation provided by BASF |
|||
Vapor Pressure | <= 0.000 bar | <= 0.000 torr | |
3M GM630 Very Soft Gripping Material 3M™ Gripping Materials are based on 3M’s proprietary micro-replicated technology. 3M gripping materials consist of a high-friction surface developed to enhance grip and reduce slippage. The plain .. |