Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 711 - 864 microns | 28.0 - 34.0 mil | Overall |
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T.. |
|||
Thickness | 711 - 864 microns | 28.0 - 34.0 mil | Overall |
Arlon 51393R032 0.032" (0.813 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: Temperature and time dependentThis data represents typical values for the production material. The data shoul.. |