Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (6 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (8 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Thickness | 8500 - 9000 microns | 335 - 354 mil | Typical free lofted thickness after heating |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |