Physical Properties Metric English Comments
Thickness 737 - 813 microns
29.0 - 32.0 mil
Overall
Arlon 55609R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThi..
Thickness 711 - 813 microns
28.0 - 32.0 mil
Overall
Arlon LW301Rxx-P1 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave
Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub..
Thickness 737 - 813 microns
29.0 - 32.0 mil
Overall
Arlon R33099G028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl..
Thickness 737 - 813 microns
29.0 - 32.0 mil
Overall
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide
Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma..