Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 205.8 - 214.2 microns | 8.102 - 8.433 mil | IEC 626 |
Dr. D. Mueller Flexiso® DMD FI 14010 00210 Polyester Electrical Insulation Structure: Flexiso® DMD, FI 14010 00210 is a flexible three layer material, consisting of a layer of polyester film, of which both sides have a layer of polyester fleece fabric and is coated with .. |