Polymer Property : Thickness = 780 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 780 - 1540 microns
30.7 - 60.7 mil
Range of Thicknesses Available
Rogers Corporation LoPro™ RO4730 Antenna Grade Non-PTFE Laminate
RO4730 LoPro Antenna Grade Laminates are fully compatible with conventional FR-4 and high temperature lead-free solder processing. The resin systems of RO4730 dielectric materials are designed to p..