Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 127 - 762 microns | 5.00 - 30.0 mil | Range of Standard Thicknesses |
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |
|||
Thickness | 660 - 762 microns | 26.0 - 30.0 mil | Overall |
Arlon 19576R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 660 - 762 microns | 26.0 - 30.0 mil | Overall |
Arlon R33920W028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: White gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, .. |