Physical Properties Metric English Comments
Thickness 724 microns
28.5 mil
Overall; Arlon SQA-TMS-003
Arlon 55629R028 0.0285" (0.724 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglassThis data repre..
Thickness 724 microns
28.5 mil
Hexcel® HexForce™ 690 Carbon Fabric
Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper..