Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55578XC028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55578XD028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers Appearance: Gray silicone gum and/or rubber on fiberglass clothThis data Represents typical values for the production ma.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon 55580R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 686 - 787 microns | 27.0 - 31.0 mil | Overall |
Arlon 55606R028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in pl.. |
|||
Thickness | 686 microns | 27.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 56586R026 0.027" (0.686 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: 1564 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clo.. |
|||
Thickness | 686 microns | 27.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 56606R026 0.027" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production materia.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon 930-125Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon 30580R030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Side 1 |
Arlon 30580R030 0.030" (0.762 mm) Uncured Unsupported Silicone Rubber on Kodacel Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Kodacel CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 686 microns | 27.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51141R027 0.0270" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PESide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values .. |
|||
Thickness | 686 microns | 27.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51581R027 0.027" (0.686 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon 930-10Xxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon LW301Rxx-P0 0.030" (0.762 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 686 - 838 microns | 27.0 - 33.0 mil | Overall |
Arlon R31551R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | >= 686 microns | >= 27.0 mil | Side 1 |
Arlon R33682C045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Infor.. |