Polymer Property : Thickness = 61.8 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 1570 microns
61.8 mil
Standard; Laminate
GrafTech GRAFOIL® GHR Standard Fluid Sealing Laminate, Metal Reinforced
GRAFOIL® Grade GHR is an uncured laminate made with GRAFOIL® Grade GTB flexible graphite adhesively bonded to both faces of a 0.002" thick flat 316 or 316L stainless steel insert. Surface iden..
Thickness 1570 microns
61.8 mil
Standard
GrafTech GRAFOIL® GHW Standard Fluid Sealing Laminate, Non-Metal Reinforced
GRAFOIL® Grade GHW is a laminate made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0025" thick high-temperature continuous woven glass fiber insert. Its functional tempera..
Thickness 1570 microns
61.8 mil
Standard
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:..
Thickness 1570 microns
61.8 mil
Standard for Double-Sided Laminate
GrafTech GRAFOIL® GRAFKOTE® Laminates, Non-Metal Reinforced
GRAFOIL® GRAFKOTE® laminates are made with GRAFOIL® Grade GTB flexible graphite thermally bonded to a 0.0005" thick polymer facing on one ("Single-Sided") or both ("Double-Sided") sides. Th..