Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1400 - 1550 microns | 55.0 - 61.0 mil | Side 1 |
Arlon 25122R060 0.060" (1.52 mm) Silicone Rubber on Laminated Fluoropolymer Film Appearance: Red silicone rubber chemically bonded to fluoropolymer filmThis data represents typical values for the production material. The data should not be used to write, or in place of, material.. |