Polymer Property : Thickness = 6.10 microns
Polymer Property :
Thickness =
6.10 microns
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Thickness
6.10
microns
0.240
mil
Special Metals Electroformed Nickel, 6 Micron (0.24 mil) Foil, As-Electroformed
Data provided by the manufacturer, Special Metals.