Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 54.9 microns | 2.16 mil | estimated wet film thickness |
Aremco Corr-Paint™ CP3015-BL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. High emissivity, inorganic black pigmented coating to 15.. |