Polymer Property : Thickness = 53.8 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 53.8 microns
2.12 mil
estimated wet film thickness
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled
Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C).