Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 47.0 - 53.0 microns | 1.85 - 2.09 mil | Total; ASTM D374 |
CEN® Electronic Material CF 200CF919 Polyimide Film CEN®CF polyimide film is the general CEN®CN film that is coated or laminated on one or both sides with Teflon® FEP fluoropolymer. CEN®CF imparts heat sealability, provides a moisture barrier, an.. |