Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 445 - 521 microns | 17.5 - 20.5 mil | Overall |
Arlon R31961R019 0.019" (0.483 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |