Physical Properties Metric English Comments
Thickness 52.1 microns
2.05 mil
ExxonMobil Escorene® LD 712.06 Film Resin  (discontinued **)
Escorene Ultra LD 712 series is a fraction melt index, 10 wt% vinyl acetate copolymer specialty film resin for applications requiring outstanding heat sealability, strength and toughness, particular..
Thickness 52.1 microns
2.05 mil
Total; ASTM D3652
3M Scotch® 3199 Security Message Box Sealing Tape
Scotch® Security Message Box Sealing Tape 3199 is a performance packaging tape used specifically where the security of the carton contents is a concern. The printed design along with the message ma..
Thickness 52.1 microns
2.05 mil
Total; ASTM D3652
3M Scotch® 311 Box Sealing Tape
Scotch® Box Sealing Tape 311 is a general purpose box sealing tape designed specifically for utility type applications on light to medium weight boxes. The product offers good performance over broa..