Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 13000 - 15000 microns | 512 - 591 mil | |
Beijing Evergrow Resources BF-15 Basalt Needle Felt Basalt fiber is a material made from extremely fine fibers of basalt. It is used as a fireproof textile in the aerospace and automotive industries and can also be used as a strengthening and repairi.. |
|||
Thickness | 13000 microns | 512 mil | |
Thermal Ceramics Kaomat 200-SL Blanket Kaomat 2000-SL silica blanket is a high temperature "shot free" amorphous silica blanket which has been heat treated during the manufacturing process to reduce residual shrinkage. This durable produ.. |
|||
Thickness | 13000 microns | 512 mil | |
Thermal Ceramics Kaomat Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |
|||
Thickness | 13000 microns | 512 mil | |
Thermal Ceramics Kaomat SL Blanket Thermal Ceramics Kaomat insulation is a non-woven needle-felted "E" fiberglass mat. Kaomat is an economical insulating material used extensively in both the marine and commercial insulation markets... |