Physical Properties Metric English Comments
Thickness 510 - 5100 microns
20.1 - 201 mil
ASTM D374
Parker Chomerics THERM-A-GAP™ G174 Cost Effective Gap Filler
Description: THERM-A-GAP™ elastomers are used to fill air gaps between PC boards or other components and heat sinks, metal enclosures, and chassis. The exceptional conformability of these advanced ..