Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 100 - 140 microns | 3.94 - 5.51 mil | |
P & P Technology NF32B050A21 Nylon/PET/Cu+Ni Conductive Fabric P & P Technology material reference NF32B050A21 is a metalised conductive fabric designed for use in EMC shielding and in the manufacture of conductive EMC gaskets. The material is a rip-stop weave .. |