Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 128 microns | 5.03 mil | estimated wet film thickness |
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C) |