Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1220 - 1320 microns | 48.0 - 52.0 mil | Overall |
Arlon LW5015Rxx-P1 0.050" (1.27 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Thickness | 1220 microns | 48.0 mil | |
3M Safety-Walk™ 710 Black Coarse Tapes and Treads Extra-large mineral particles and durable construction provide additional slip resistance in extreme conditions.For extreme, heavy traffic areasExtra-large abrasive mineral particles help provide a .. |
|||
Thickness | 1220 microns | 48.0 mil | |
3M Safety-Walk™ 770 Gray Coarse Tapes and Treads Extra-large mineral particles and durable construction provide additional slip resistance in extreme conditions.For extreme, heavy traffic areasExtra-large abrasive mineral particles help provide a .. |