Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1190 microns | 47.0 mil | |
Rogers Corporation Poron® 4701-30-25047 P Urethane Foam, Very Soft, Supported with Clear Polyester Film Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Thickness | 1190 - 1350 microns | 47.0 - 53.0 mil | Overall |
Arlon LW5015Rxx-P0 0.050" (1.27 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |